Test | Test Method | Requirement |
Tensile strength | ASTM D 2671 | >11MPa |
Elongation at break | ASTM D 2671 | >400% |
Elongation at break after heat aging | ASTM D 2671 | >300% |
Volume resistivity | IEC 93 | 1013Ω.cm |
Dielectric strength | IEC 243 | >15KV/mm |