Test | Test Method | Requirement |
Tensile strength | ASTM D 2671 | ≥12 Mpa |
Elongation at break | ASTM D 2671 | >400% |
Tensile strength after heat aging | ASTM D 2671/120℃,168h | ≥8.5 Mpa |
Elongation at break after heat aging | ASTM D 2671/120℃,168h | ≥200% |
Volume resistivity | IEC 93 | 1013Ω.cm |
Dielectrical strength | IEC 243 | ≥15KV/mm |
Flame retardancy (oxygen index) | ASTM 4589 | ≥25 |
Water absorption rate | ISO 62/23℃,14 days | ≤1% |
Type |
Model number |
Expanded (mm) |
Recovered(mm) |
|||||||
D1(Min) |
D2(Min) |
D1(Max) |
D2(Max) |
L1(±10%) |
L2(±10%) |
L(±10%) |
W1(±10%) |
W2(±10%) |
||
Right Angle |
SHMR-1(80/36-35-18) |
80 |
35 |
36 |
18 |
170 |
125 |
- |
4.2 |
3.5 |
SHMR-2(80/36-50/18) |
80 |
50 |
36 |
18 |
170 |
125 |
- |
3.8 |
3.5 |
|
SHMR-3(95/38-70/28) |
95 |
70 |
38 |
28 |
160 |
140 |
- |
4.2 |
4.8 |
|
Straight |
SHMR-4(80/35-34/20) |
80 |
34 |
35 |
20 |
145 |
30 |
220 |
3.2 |
3.2 |
SHMR-5(80-35/58-20) |
80 |
58 |
35 |
20 |
145 |
30 |
220 |
3.2 |
3.2 |